High magnetization FeCo nanoparticles for magnetorheological fluids with enhanced responseEgilea (beste erakunde batekoa)
Beste instituzio
Universidad del País Vasco/Euskal Herriko Unibertsitatea (UPV/EHU)Centro de Física de Materiales (CFM) (CSIC–UPV/EHU)
Bertsioa
Postprinta
Eskubideak
© 2021 Royal Society of ChemistrySarbidea
Sarbide irekiaArgitaratzailearen bertsioa
https://doi.org/10.1039/D0SM01702GNon argitaratua
Soft Matters Vol. 17. N. 4. Pp. 840-852, 2021Lehenengo orria
840Azken orria
852Argitaratzailea
Royal Society of ChemistryLaburpena
We present results concerning the fabrication of a new magnetorheological fluid with FeCo magnetic nanoparticles (NPs) as magnetic fillers. These NPs have been fabricated by using the chemical reducti ... [+]
We present results concerning the fabrication of a new magnetorheological fluid with FeCo magnetic nanoparticles (NPs) as magnetic fillers. These NPs have been fabricated by using the chemical reduction technique and show a pure crystalline phase with size ranging among 30–50 nm and high magnetization, 212 ± 2 A m2 kg−1. They agglomerate due to the strong magnetic dipolar interaction among them. These FeCo nanoparticles were used to synthesize a magnetorheological fluid by using oleic acid as surfactant, mineral oil as carrier liquid and Aerosil 300 as additive to control the viscosity of the fluid. The synthesized fluid showed a strong magnetorheological response with increasing shear stress values as the magnetic field intensity increases. Thus, we have measured a superior performance up to 616.7 kA m−1, with a yield stress value of 2729 Pa, and good reversibility after demagnetization process. This value competes with the best ones reported in the most recent literature. We have compared the obtained results with our previous reported ones by using high magnetization Fe NPs fabricated by the electrical explosion of wire method (Fe-EEW). [-]