Thermal Mass Effect on the Solution Cooling Rate and on HIPped Astroloy Component Properties
(MDPI, 2022)Astroloy is a Ni-based superalloy with high-volume fraction of γ′, which gives high temperature properties but reduces its forgeability. Therefore, powder metallurgy manufacturing processes such as Near Net Shape HIPping ...