Crystal-plasticity-finite-element modeling of the dynamic response of a directionally solidified nickel-based superalloy
(2020)The flow stress behaviour of a directionally solidified nickel-base superalloy,MAR-M247, is presented through the combination of experiments and crystal-plasticity simulations.The experimental campaign ...